Yog Dab Tsi Hlau Txiav Edm?

Jul 22, 2020 Tso lus

Lub conductivity ntawm dej yog tswj tau zoo thiab lub txim tau tswj xyuas kom zoo thiab muaj nyob kom nws tsuas cuam tshuam rau thaj chaw ntawm cov khoom. Qhov no muab ib puag ncig zoo rau EDM txheej txheem thiab ua rau muaj kev nce qib ntawm ua tau zoo.

EDM yog cov txheej txheem uas tsis yog ib txwm muaj nyob rau hauv uas cov ntaub ntawv conductive raug txiav rau hauv hluav taws xob tooj liab lossis tooj dag hlau siv hluav taws xob. Cov Hluav Taws Xob Hluav Taws Xob Hluav Taws Xob (WEDM) siv cov xov tooj hlau rau" txiav" lossis teeb tsa ib qho chaw ua haujlwm (feem ntau cov khoom siv coj los ua) rau hauv cov xaim hluav taws xob me uas ua raws li ib txog kev. Kuj hu ua hlau txiav, hlau xaim tawm lossis xaim txiav, nws tseem paub los ntawm nws lub npe hu ua xaim hluav taws xob hluav taws xob (EED).

Nyob rau hauv cov hlau EDM, cov xov hlau nqa ib sab ntawm tus nqi hluav taws xob, thiab tus neeg nqa khoom nqa lub luag haujlwm ntawm lwm sab. Thaum cov hlau xaim los ze rau qhov sib txuas, qhov kev nyiam ntawm cov nqi hluav taws xob ua rau muaj hluav taws xob tswj uas ua kom yaj lossis evaporates microscopic particles hauv cov khoom.

Hlau EDM txiav cov khoom siv conductive nrog hluav taws xob tam sim no, tsim kom muaj cov npoo du uas tsis tas yuav tsum tau txhim kho ntxiv lossis polishing. Cov txheej txheem no yog siv los txiav cov paib, xuas nrig ntaus tuag thiab tuag uas ua los ntawm cov ntaub ntawv uas ua tiav, suav nrog carbides, uas nyuaj rau tshuab nrog rau lwm txoj kev, xws li hlau. Nyias cov hlua ntawm cov hlau hlau yog dhau los ntawm kev txiav cov phaj ntawm tus nqi ntawm txog 1,000 volts rau ib square nti (0.5 millimeters ib ob).

X - Y dav hlau, tswj los ntawm CNC, cov lus qhia tuaj yeem txav mus rau ob txoj kev qhia: nce thiab nqis. Cov lus qhia sab saud tuaj yeem tswj tau qhov txav ntawm off-axis thiab txav nws nce los yog nce, tsim kom muaj peev xwm txiav cov ntsia hlau los yog hloov cov duab. Cov xov hlau EDM (WCEDM) coj hluav taws xob tam sim no ntawm cov xov hlau tsis sib haum uas ua raws li cathodes thiab coj cov kev xav txiav (kerfs).

Qhov nce siab ntxiv no tso cai rau kev txiav txim siab peb-ntu thiab muab lub phaj ua ntu ntev rau kev tshem tawm nrog rau kev muaj peev xwm rov kho qhov loj thiab cov qauv ntawm cov xov hlau.

Thaum lub tshuab ua kom zoo nkauj tsis ib txwm tsim cov fab fab me lossis cov qauv ntau dhau los, qhov muaj zog ntawm ED-M xaim ua rau ntau cov qauv txiav. SinkerEDM, tseem hu ua dive, siv cov xov hlau ntawm cov duab sib txawv thiab ntau thiab tsawg, nrog rau ntau hom kev cuam tshuam, kom tshem cov khoom tawm ntawm qhov chaw ua haujlwm. Lub xov hlau txiav cov cuab yeej ua haujlwm nrog lub koos pij tawj tswj cov lej ua haujlwm (CNC) uas tuaj yeem tswj cov xov hlau ntawm ntau txoj hau kev, yog li muab qhov yooj yooj yim dua.

Cov hluav taws xob hluav taws xob feem ntau yog ua los ntawm graphite, tab sis lwm cov ntaub ntawv xws li tooj liab, npib tsib xee, tooj liab oxide lossis lwm yam hlau kuj tseem siv. Cov yam ntxwv geometric ntawm cov electrodes tuaj yeem kho kom tau raws li qhov xav tau ntxiv.

Hlau Hlais Hluav Taws Xob Kev Ntsuam Cov Hluav Taws Xob yog qhov zoo tshaj plaws rau kev ua haujlwm qhov hluav taws xob xeb siv hluav taws xob. Workpiece thiab cov electrodes tau raus hauv cov kua hluav taws xob dielectric (cov roj lossis cov roj hluavtaws) thiab lub tshuab ua haujlwm ncaj qha cov hluav taws xob rau cov khoom siv ua haujlwm siv CNC thev naus laus zis. Nyob rau hauv cov hlau EDM, lub zog ntawm hluav taws xob txhawm los ntawm kev thaiv txoj kab nruab nrab ntawm cov kua raug xaiv thaum lub electrode mus rau qhov chaw ua haujlwm. Ib lub txim taws yog tsim thaum cov khoom me me ntawm cov khoom yaig me me los ntawm kev ua kom yaj lossis yaj.

Hlau EDM pabcuamfeem ntau siv rau kev txiav carbides uas qee zaum nyuaj rau kev kho nrog lwm txoj kev txiav. Zoo meej ncaj thiab burr - dawb machining yuav ua tiav nrog WireEDM machining.

Los ntawm kev txiav cov kev ntxhov siab ntawm cov khoom siv, cov hlau tsis tshua muaj neeg hlau tuaj yeem tsim tau yam tsis muaj kev xav tau ntxiv cov cuab yeej lossis cov cuab yeej xws li kev xyaum.

Hlau EDM tso cai rau siv cov khoom siv tawv, thim thiab tawg uas yog xaim hluav taws xob. Los ntawm kev siv hluav taws xob tso tawm hluav taws xob los ntawm cov xov hlau zoo, Cov tshuab hlau hlau muaj peev xwm txiav tau qhov meej thiab ua kom muaj cov duab. Qhov no muaj nws qhov tsis zoo, txawm li cas los xij, vim tias qhov cuam tshuam tuaj yeem tsim kev ntxhov siab uas cuam tshuam cov khoom thaum lub sijhawm txiav thiab ua rau cov cuab yeej hnav kom nrawm.

Thaum cov xov hlau tuaj yeem tsim qhov tsis muaj qhov sib txawv ntawm cov duab sib txawv, txawm tias cov kab sib txawv me me thiab cov qhov tuaj yeem tsim thaum cov khoom siv ua kom sov, muag muag thiab tawv.

Txhawm rau ua cov hlau EDM hlau muaj peev xwm ua qhov no, quab yuam yuav tsum tau siv rau ntu ntawm lub sijhawm. Hlau EDD cov dej num tuaj yeem tsim teeb tsa thiab ua tiav hauv sijhawm tsawg dua, txhais tau tias koj tuaj yeem tau txais cov khoom tseem ceeb kom nrawm dua.