kub chamber tuag-casting cov khoom yog ib tug high-precision, complex, nyias-walled, high-lub zog, high-corrosion-resistant tivthaiv uas yog tuag-cam khwb cia los ntawm ntau yam aluminium alloys, magnesium alloys, zinc alloys, thiab lwm yam ntaub ntawv casting. Vim tias cov khoom siv kub kub tuag casting muaj cov yam ntxwv ntawm kev kub siab, kev kub ceev, kev ua haujlwm siab, thiab kev ua haujlwm siab, nws muaj ntau yam kev siv thiab tuaj yeem siv rau hauv kev tsim tsheb, hluav taws xob, kev lag luam tub rog, aerospace, computers. , thiab lwm yam.

Kub Chamber Tuag Casting Qhov Zoo
- Kev ua tau zoo ntau lawm: Lub tshuab melting rauv thiab cov khoom siv tuag-casting siv nyob rau hauv kub chamber tuag-casting txoj kev yog khiav ib txhij tsis reheating, thiab cov raw khoom siv tus nqi yog siab, uas yuav ho txhim khu ntau lawm efficiency.
- High casting nto zoo: Vim hais tias lub pas dej molten hlau tsis tuaj rau hauv cov huab cua thoob plaws hauv cov txheej txheem compression, tsis muaj oxidation los yog porosity ntawm lub casting qhov chaw, thiab cov nto zoo heev.
- High-casting precision: Kub chamber tuag casting muaj qhov siab precision casting, tso cai rau nws ua cov khoom nyuaj nrog qhov pom qhov tseeb qhov tseeb thiab nto polished.
- Khoom siv ntau yam: kub chamber tuag casting tuaj yeem siv ntau yam ntawm cov ntaub ntawv hlau thiab ua castings ntawm ntau hom thiab kev siv.
- Ib puag ncig kev tsim khoom zoo: Tsis zoo li cov thev naus laus zis thev naus laus zis thev naus laus zis, kub chamber tuag-casting tsis xav tau cov neeg ua haujlwm nrhiav haujlwm ua haujlwm hauv qhov kub thiab txias. Qhov chaw casting yog qhov tsim nyog ruaj khov thiab noj qab nyob zoo rau cov neeg ua haujlwm.
- pheej yig casting nqi: Txawm hais tias kub chamber tuag casting muaj tus nqi pib peev, tus nqi siv raw khoom yog siab, thiab tus nqi ntawm castings feem ntau pheej yig.
Ua cov kauj ruam ntawm kub chamber tuag-casting khoom
- Pwm tsim thiab tsim khoom: Ua ntej, pwm tsim thiab tsim khoom yuav tsum tau ua raws li tus qauv tsim ntawm cov khoom. Qhov zoo ntawm cov pwm yuav cuam tshuam ncaj qha rau kev ua haujlwm zoo ntawm cov khoom.
- Kub chamber tuag casting: Lub preheated aluminium alloy kua hlau yog txhaj rau hauv pwm, thiab casting yog tsim los ntawm high-pressure txhaj. Qhov zoo ntawm kub chamber tuag casting yog ceev ceev, high efficiency efficiency, siab nto tiav thiab siab qhov tseeb ntawm castings.
- Kev kho de-flash: Feem ntau muaj qee qhov tsis xws luag ntawm qhov chaw ntawm aluminium alloy castings, nrog rau qhov pores, shrinkage kab noj hniav, pinholes, loj nplej, thiab lwm yam, uas yuav tsum tau de-flashed. Cov txheej txheem ntawm kev kho flashing muaj xws li txhua yam flashing, sib tsoo log flashing, oxidation flashing, thiab lwm yam.
- Machining: Raws li qhov yuav tsum tau ua ntawm cov khoom, machining yog nqa tawm, feem ntau suav nrog tig, milling, drilling, tapping, thiab lwm yam.
- Kev kho deg: Kev kho deg ntawm castings, xws li sandblasting, polishing, anodizing, electroplating, thiab lwm yam.
- Kev soj ntsuam zoo: Ua kom muaj kev soj ntsuam zoo ntawm cov khoom ua tiav, suav nrog kev tshuaj xyuas qhov tseeb ntawm qhov tseeb, zoo li zoo, cov khoom muaj pes tsawg leeg, thiab lwm yam.
- Kev sib dhos: Sib sau ua ke raws li qhov yuav tsum tau ua ntawm cov khoom, suav nrog vuam, ntsia hlau txuas, sib txuas, thiab lwm yam.
- Packing: Pob raws li qhov yuav tsum tau muaj ntawm cov khoom, uas yog yooj yim rau kev thauj mus los thiab cia.
Daim ntawv thov
Kub chamber tuag-casting cov khoom yog ib tug high-precision thiab high-complexity casting txheej txheem, mas siv nyob rau hauv tsheb, electronics, machinery, kev sib txuas lus, railways, aerospace, thiab lwm yam industries, rau zus tau tej cov complex aluminium alloys, magnesium alloys, zinc. Alloy, thiab lwm yam, xws li automotive engines, log, gearboxes, chassis Cheebtsam, electronics chassis, electronics, thiab lwm yam.